Please use this identifier to cite or link to this item: http://dr.iiserpune.ac.in:8080/xmlui/handle/123456789/9517
Full metadata record
DC FieldValueLanguage
dc.contributor.authorChoudhari, Sanjuen_US
dc.contributor.authorKEDIA, DINESH KUMARen_US
dc.contributor.authorYadav, Manishaen_US
dc.contributor.authorRam, Puraen_US
dc.date.accessioned2025-04-15T06:51:46Z-
dc.date.available2025-04-15T06:51:46Z-
dc.date.issued2024-11en_US
dc.identifier.citationJournal of the Indian Chemical Society, 101(11), 101351.en_US
dc.identifier.issn0019-4522en_US
dc.identifier.urihttps://doi.org/10.1016/j.jics.2024.101351en_US
dc.identifier.urihttp://dr.iiserpune.ac.in:8080/xmlui/handle/123456789/9517-
dc.description.abstractTin Sulfide (SnS) has recently garnered significant attention due to its impressive Seebeck coefficient and low thermal conductivity. However, its electrical performance is notably poor, necessitating appropriate doping for its enhancement. To address this, we employed the conventional hydrothermal method to synthesize polycrystals of pristine and lead (Pb)-doped SnS samples to observe the impact on thermoelectric parameters. Utilizing FESEM, we obtained sheet sizes on the nanometer scale and observed irregular sheet-type morphology. HRTEM analysis confirmed the polycrystalline nature of the synthesized samples. Thermal stability assessment through thermogravimetric analysis (TGA) was conducted on all samples up to a temperature of 600 °C. The hydrothermal method resulted in nanostructuring that effectively suppressed the thermal conduction of low-frequency phonons, with increased phonon scattering attributed to the small grain size of particles. For pristine SnS nanoparticles, we determined the lowest total thermal conductivity (κT) to be 0.18 W (m-K)−1, and the highest Seebeck coefficient reached 412.71 μVK−1 at 620 K. In the case of the SnS–Pb(3 wt%) doped sample, there was a slight reduction in the total thermal conductivity (κT) compared to the pristine SnS sample. The pristine SnS sample exhibited the highest electrical conductivity (σ) of 0.21 S/cm at 620 K. In contrast, the SnS–Pb(3 wt%) doped sample demonstrated a twofold increase in electrical conductivity, measuring 0.38 S/cm at 620 K. This enhancement can be attributed to the increased carrier concentration resulting from the Pb(3 wt%) doping of SnS.en_US
dc.language.isoenen_US
dc.publisherElsevier B.V.en_US
dc.subjectConventional hydrothermal methoden_US
dc.subjectPb-doped SnSen_US
dc.subjectLow thermal conductivityen_US
dc.subjectSeebeck coefficienten_US
dc.subject2024en_US
dc.titleThermoelectric properties of polycrystalline pristine and Pb-doped SnS materials using a conventional hydrothermal methoden_US
dc.typeArticleen_US
dc.contributor.departmentDept. of Physicsen_US
dc.identifier.sourcetitleJournal of the Indian Chemical Societyen_US
dc.publication.originofpublisherForeignen_US
Appears in Collections:JOURNAL ARTICLES

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.